@inbook{f39eae2ed456400d928c7e0f476199ca,
title = "Bulk and surface analysis of carbonaceous materials",
author = "Shuttleworth, {Peter S.} and Niki Baccile and White, {Robin J.} and Eric Nectoux and Budarin, {Vitaliy L.}",
year = "2015",
month = feb,
day = "20",
doi = "10.1039/9781782622277-00311",
language = "English",
isbn = "978-1-84973-832-3",
series = "RSC Green Chemistry",
publisher = "The Royal Society of Chemistry",
pages = "311--354",
editor = "White, {Robin J. }",
booktitle = "Porous Carbon Materials from Sustainable Precursors",
address = "United Kingdom",
}